Futamura cuts cellulose film carbon footprint by 24%
发布时间:2026-10-20 | 来源:Bioplastics Magazine | 作者:Bioplastics Magazine
Futamura (Wigton, UK) is proud to announce significant progress in reducing the carbon footprint of its cellulose films
Since 2019, Futamura has delivered a cumulative carbon saving equivalent to removing ~70,000 cars from UK roads for an entire year. This figure represents avoided CO₂e emissions associated with lacquered (based on NatureFlexT ™ NVS) and plain film production between 2019 and 2025, calculated using IPCC AR6 GWP100 values from an independent third-party life cycle assessment from ERM. This resulted in an average reduction of 24% of the carbon footprint of their NatureFlex films (The calculation is based on the difference in the carbon footprint between 2019 and 2025. Based on this, the actual amount of CO2e saved was ~100,000 tonnes). Building on this success, additional major investments are now underway and scheduled for implementation by 2027/28. One example is the recently announced, internally known, Wet Sulphuric Acid (WSA) project. The installation will divert waste gases from the production process to generate a valuable raw material via an oxidation process. Heat generated as a byproduct of the chemical reaction will then be used to generate steam, the main form of energy utilised in the production process. Once operational, this asset will generate 15% of the total energy requirement of the Futamura site. These investments are projected to reduce Futamura’s CO₂e emissions even further, the equivalent to removing an additional ~4,000 cars from UK roads every year (based on 2025 production volumes). This represents another major step in reducing the carbon footprint of their products. A key contributor to recent carbon reductions has been the investment in a new, high-performance compressed air system to strengthen their energy efficiency, reduce carbon emissions, and improve operational resilience. An independent air survey confirmed that this new system is outperforming expectations. To further enhance the sustainability, Futamura integrated a heat-recovery system utilising waste heat from the compressors to pre-heat their thermotanks, this reduces the steam…
返回资讯频道