Transforming a soybean processing byproduct into a material for skin protection and repair is the prospect outlined by a study that used okara, a residue from t

Transforming a soybean processing byproduct into a material for skin protection and repair is the prospect outlined by a study that used okara, a residue from the production of tofu and soy-based beverages, to obtain a bioactive, biodegradable, 3D-printable biomaterial.