发布时间:2026-10-23 | 来源:Nature Scientific Reports | 作者:Qiukai Qi

Edible transient robots can be eaten, digested, and metabolized by human, and are a rapidly emerging technology towards sustainable autonomous robotics. Among n

Edible transient robots can be eaten, digested, and metabolized by human, and are a rapidly emerging technology towards sustainable autonomous robotics. Among numerous developments of edible robotic components, edible tilt sensors can inform the self state of the robot such as orientation and tilt angle, representing a key technology for autonomous robotic control. However, the only existing fully edible tilt sensor in the literature generates binary output and is hard to monitor the continuous inclination angle change. Additionally, the resistive sensing principle is strongly affected by heat and humidity, hindering its application to wet environments such as in the human body. To bridge the gap, we present the first edible tilt sensor capable of monitoring continuous change of tilt angle. Our tilt sensor is based on capacitance variance, which by principle minimizes the effects of temperature and humidity. The sensor is composed of a gelatine compartment coated with wax, graphite electrodes and an edible dielectric sensing liquid. We present the concept, design, fabrication, and characterization of our sensor, and demonstrate its application in robotic control. The sensor has a large working range (0 \(^\circ\) to 80 \(^\circ\) ) with a high sensitivity (2.34 %/ \(^\circ\) ) and repeatability. This device paves the way for future development of sustainable autonomously navigable edible soft robotics.

返回资讯频道