AI-powered robotic laboratory paves the way for discovering next-generation heat-resistant coatings

发布时间:2026-10-26 | 来源:Phys.org 材料与聚合物 | 作者:Phys.org 材料与聚合物

Researchers have developed a self-driving laboratory that combines artificial intelligence and robotics to automate laboratory tasks, from accurately measuring

Researchers have developed a self-driving laboratory that combines artificial intelligence and robotics to automate laboratory tasks, from accurately measuring and mixing chemical ingredients to high-temperature furnace processing and sample retrieval.