Flexible Surface Acoustic Wave Sensor Based on an SXFA Sensitive Film for DMMP Detection

发布时间:2026-10-26 | 来源:MDPI Polymers | 作者:Cancan Yan, Yanze Wang, Junchao Yang, Jie Yang, Lin Zhang, Yong Pan, Genwei Zhang

Rapid and reliable detection of organophosphorus nerve agents is essential for public safety and individual protection. In this work, a flexible surface acousti

Rapid and reliable detection of organophosphorus nerve agents is essential for public safety and individual protection. In this work, a flexible surface acoustic wave (SAW) gas sensor based on a hexafluoroisopropyl (HFIP)-functionalized polysiloxane (SXFA) sensitive film was developed for the detection of dimethyl methylphosphonate (DMMP), a widely used simulant of sarin (GB). SXFA was synthesized through a two-step route and systematically characterized by Fourier-transform infrared spectroscopy (FTIR), 1H/19F/13C nuclear magnetic resonance (NMR), gel permeation chromatography (GPC), differential scanning calorimetry (DSC), thermogravimetric analysis (TGA) and scanning transmission electron microscopy coupled with energy-dispersive X-ray spectroscopy (STEM/EDX). The results confirm the successful incorporation of HFIP groups and reveal a low glass-transition temperature (Tg = −23.5 °C, ΔCp = 0.295 J·g−1·K−1), a weight-average molecular weight of ~3200 g·mol−1, a thermal-stability limit of ~200 °C, and a characteristic HFIP side-chain cleavage at 343.4 °C with a final residue of 18.37%. The flexible device consisted of a polyimide (PI) substrate, a magnetron-sputtered AlN piezoelectric layer and silver interdigital transducers (IDTs) and operated at a center frequency of ~200 MHz; a rigid quartz-based delay line was used as a reference. The dependence of the insertion loss (IL) on film thickness was described by a third-order polynomial (R2 = 0.960), from which an optimal thickness window of 150–450 nm was identified, and 450 nm gave the best gas-sensing performance (response 23.5 mV at 3 mg·m−3 DMMP, IL −16.0 dB; mean ± SD, n = 3 independently prepared devices per thickness). The optimized sensor exhibited a linear response to DMMP from 0.4 to 6 mg·m−3 (y = 30.88x + 8.988, R2 = 0.9985) at 28.1 °C, fast response and recovery (~75 s each), excellent reproducibility (relative standard deviation, RSD = 0.50%, n = 7), pronounced selectivity towards DMMP and DFP over com…

返回资讯频道