Yeast paired with electricity can convert CO₂ into a chemical used in biodegradable plastics

发布时间:2026-10-28 | 来源:Phys.org 材料与聚合物 | 作者:Phys.org 材料与聚合物

To limit further climate change, researchers are exploring technologies that can convert atmospheric carbon dioxide (CO₂) into useful products. In collaboration

To limit further climate change, researchers are exploring technologies that can convert atmospheric carbon dioxide (CO₂) into useful products. In collaboration with BOKU University in Vienna (Austria), researchers at the Helmholtz Centre for Environmental Research (UFZ) have demonstrated that electrochemical and microbial processes can be combined to capture CO₂ and produce itaconic acid, a bio-based chemical used in industry. According to the researchers, this new process demonstrates how CO₂ emissions can be converted into sustainable bio-based products, with the potential to produce a wider range of valuable chemicals by using different microorganisms.