Response Surface Optimization of Water-Based Drilling Mud Viscosity Using Titanium Dioxide–Graphene Oxide Nanocomposite and Sodium Alginate Biopolymer
发布时间:2026-10-27 | 来源:MDPI Polymers | 作者:Jianlong Wang, Ren Wang, Muhammad Arqam Khan, Qibing Wang, Shaine Mohammadali Lalji, Jianwei Liu, Ha
Drilling fluids play a critical role in efficient cuttings transport, suspension of drilled solids, hydraulic performance, and wellbore stability, making rheolo
Drilling fluids play a critical role in efficient cuttings transport, suspension of drilled solids, hydraulic performance, and wellbore stability, making rheological control essential for safe and efficient drilling operations. However, conventional viscosifiers may have limited performance under demanding drilling conditions, motivating the development of nanocomposite–polymer systems with enhanced rheological tunability. The work in this article explores the viscosities of drilling fluid following the incorporation of a hydrothermally synthesized nanocomposite material formed through the interaction of titanium and graphene oxide, and a biopolymer, sodium alginate. A response surface methodology (RSM) approach based on concentration was employed to systematically observe the effects of these two different entities on the viscosity of the drilling fluid. During testing, 13 experimental runs were conducted to assess the influence of particle concentration on plastic viscosity and apparent viscosity. A strong correlation was established between the experimental test runs and the predictive model generated using this RSM, with R2 = 96.30% (adjusted R2 = 93.65% and predicted R2 = 84.13%) for plastic viscosity and R2 = 96.97% (adjusted R2 = 94.80% and predicted R2 = 85.04%) for apparent viscosity, and all 95% relative errors below 15%. ANOVA showed that the nanocomposite concentration was the significant parameter with p-value 0.05. Increasing the nanocomposite from 0.35 to 3.5 g at 0.35 g of sodium alginate raised the predicted plastic viscosity from 9.55 to 23.95 cP (+150%) and the apparent viscosity from 18.83 to 38.03 cP (+101%). The graphene oxide provides the anchoring sites to TiO2 nanoparticles that ultimately increase the inter-particle contact and exert an influence on both the viscosities. Additionally, in aqueous media, TiO2 nanoparticles hydroxylate, thus forming hydrogen bonding with graphene oxide. This interaction reduces the slippage effect of TiO2 nano…
返回资讯频道