Wax-Functionalized Bacterial Cellulose Foils as Renewable Food Packaging with Enhanced Barrier and Antimicrobial Performance
发布时间:2026-11-01 | 来源:MDPI Polymers | 作者:Elżbieta Redlarska, Klaudia Snopek, Martyna Mielniczuk, Karol Fijałkowski, Anna Żywicka
The study aims to develop a novel, fully biodegradable food-packaging material made from bacterial cellulose (BC) films coated with natural waxes. BC films (BCF
The study aims to develop a novel, fully biodegradable food-packaging material made from bacterial cellulose (BC) films coated with natural waxes. BC films (BCFs) were produced by Komagataeibacter xylinus biosynthesis, then purified, homogenized, and dehydrated. To boost water resistance and bioactivity, each film was coated with one of twelve plant- or animal-derived waxes, without harsh solvents or added waste. Wax coating markedly enhanced barrier and mechanical performance and transformed the BCF surface into a highly hydrophobic layer, slashing water uptake and permeability versus uncoated films. Moreover, BCF coated with waxes (BCF-Ws) showed potent antimicrobial and antibiofilm activity against Gram-positive Staphylococcus aureus, Gram-negative Escherichia coli, and yeast Candida albicans. The rapeseed-coconut wax exhibited the most potent broad-spectrum antimicrobial activity, while laurel, candelilla, coconut, carnauba, rapeseed, and bees waxes also demonstrated strong inhibitory effects against Staphylococcus aureus and Candida albicans. As a proof of concept, we wrapped ham, bread, cheese, and fruit in BCF coated with rapeseed-coconut wax and observed substantially lower microbial growth than with conventional packing materials. These results position BC-Ws composites as promising, eco-friendly alternatives for active food packaging with superior barrier and antimicrobial properties.
返回资讯频道