Polymer interface-driven perovskite crystallization in electrospun fibers

发布时间:2026-10-29 | 来源:OpenAlex | 作者:Mia Klopfenstein; Shlok Joseph Paul; Arnold Wijoyo; Pulkita Jain; Eray S. Aydil; Ayaskanta Sahu; Tse

Polymer incorporation into metal halide perovskite films is an effective strategy to control perovskite nucleation and crystallization, passivate defects and su

Polymer incorporation into metal halide perovskite films is an effective strategy to control perovskite nucleation and crystallization, passivate defects and suppress humidity-induced degradation. In this work, we use enthalpic interactions between insulating polymers and formamidinium lead iodide (FAPbI 3 ) to control FAPbI 3 crystal size, quality and location. Specifically, we electrospin interconnected networks of FAPbI 3 precursor/poly(vinylpyrrolidone) (PVP) composite nanofibers, then encapsulate the fibers in a poly(methyl methacrylate) (PMMA) or poly(phenylene oxide) (PPO) scaffold prior to thermal annealing to induce α-FAPbI 3 crystallization. Polar PMMA nucleated dense, polycrystalline FAPbI 3 crystals at the PMMA/fiber interface. Non-polar PPO scaffolds, on the other hand, suppressed FAPbI 3 nucleation at the interface, suggesting enthalpically unfavorable perovskite-polymer interactions. Transmission electron microscopy revealed that PPO drives FAPbI 3 crystallization within fiber interiors to form FAPbI 3 core/PVP shell structures. PPO-confined FAPbI 3 fibers exhibited long excited carrier lifetimes of ~1200 ns, surpassing those of bulk single crystals, but poor charge transfer to a hole transport layer due to the presence of an insulating PVP shell. Unconfined and PMMA-confined FAPbI 3 fibers, in contrast, showed rapid, defect-induced photoluminescence decay and fast charge transfer, the latter of which contributed to improved photodetector responsivity compared to PPO-confined fiber photodetectors. Polymer incorporation into these perovskite films improved their environmental stability, with α-FAPbI 3 persisting for more than seven weeks of storage in air. Collectively, these results demonstrate the use of perovskite-polymer interactions to dictate perovskite crystallization outcomes, including size, location and defect density.

返回资讯频道