Interphase Engineering of Epoxy/Wool Biocomposites via Lignin Coating: Effects on Mechanical and Hygrothermal Performance
发布时间:2026-11-05 | 来源:MDPI Polymers | 作者:Alessia Pantaleoni, Baljinder K. Kandola, A. Richard Horrocks, Irene Bavasso, Maria Paola Bracciale,
This work has investigated epoxy composites reinforced with wool fabrics modified by an organosolv lignin coating deposited via a sustainable protocol. The lign
This work has investigated epoxy composites reinforced with wool fabrics modified by an organosolv lignin coating deposited via a sustainable protocol. The lignin layer was introduced to tailor the fiber/matrix interphase, aiming to improve adhesion and reduce water-related degradation associated with the intrinsic hygroscopicity of wool. Laminates were manufactured by vacuum-assisted resin transfer molding (VARTM) and systematically characterized. Thermogravimetric analysis demonstrated improved thermal stability and higher char yield in lignin-coated composites. Mechanical tests revealed enhanced flexural strength (+21%) and modulus (+31%), together with a modest increase in interlaminar shear strength. SEM analysis of the fracture surfaces provided additional evidence of changes in fiber–matrix interfacial interactions. Low-velocity impact and DMA results further supported the role of the coating in improving load transfer and viscoelastic response. Water absorption tests indicated reduced equilibrium uptake and slower diffusion kinetics, highlighting the hydrophobic barrier function of the lignin layer. Collectively, these results show that the lignin coating acts primarily as an interphase modifier and water-barrier layer, enabling low-value wool fabrics to be upgraded into functional reinforcements for more durable epoxy biocomposites.
返回资讯频道