Synthesis and Characterization of a Propolis-Containing Cellulosic Textile Functionalized with a Crosslinked Agar/κ-Carrageenan Biopolymer Network: Structure–Property Relationships and In Vitro Biological Responses
发布时间:2026-11-08 | 来源:MDPI Polymers | 作者:Yassine El‐Ghoul, Sami M. Alharbi, Suliman S. Aba-alkhayl, Béchir Hammami
The development of multifunctional wound dressings based on bioactive polymers offers an opportunity to combine moisture management, structural stability, and b
The development of multifunctional wound dressings based on bioactive polymers offers an opportunity to combine moisture management, structural stability, and biological functionality within a single material. However, the integration of crosslinked agar/κ-carrageenan coatings, a poly(acrylic acid)/sodium hypophosphite (PAA/SHP) crosslinking system, and propolis on cellulosic textile substrates, together with the relationships between material properties and in vitro biological responses, warrants further investigation. In this study, a functionalized cellulosic textile incorporating agar, κ-carrageenan, PAA, SHP, and propolis (PS) was prepared and characterized. The curing conditions of 140 °C for 15 min were selected based on previous work and adopted in the present study. The resulting materials were characterized by ATR-FTIR spectroscopy, scanning electron microscopy (SEM), swelling measurements, and tensile testing. The functionalized textiles exhibited a mass gain of 23.03% and a swelling ratio of 630%, indicating substantial material incorporation and water uptake. The wet breaking force reached 4.89 N, demonstrating measurable mechanical performance under hydrated conditions. ATR-FTIR findings were consistent with chemical interactions associated with the proposed PAA-mediated crosslinking mechanism, while SEM revealed morphological features consistent with the formation of a polymeric coating on the cellulose fibers. The complete formulation exhibited an apparent relative HepG2 MTT response of 132.5% after 72 h, indicating metabolic activity above that of the control under the tested conditions. The propolis-containing materials also exhibited antibacterial activity against the Gram-positive bacterium Staphylococcus aureus and the Gram-negative bacterium Escherichia coli, with inhibition zones of 39.2 mm and 29.3 mm, respectively, and demonstrated antifungal activity against Candida albicans. Further evaluation using MCF-7 breast cancer cells and non-tumori…
返回资讯频道