CDEF-Tg: Machine Learning-Based Descriptor–Embedding Fusion for Glass Transition Temperature Prediction in a Polyimide-Oriented Polymer Dataset
发布时间:2026-11-07 | 来源:MDPI Polymers | 作者:Mücahit Çalışan, İbrahim Ayaz
Predicting the glass transition temperature (Tg) of polymers from structures remains difficult, and whether descriptors and molecular-language embeddings carry
Predicting the glass transition temperature (Tg) of polymers from structures remains difficult, and whether descriptors and molecular-language embeddings carry complementary information is unclear. CDEF-Tg (Compact Descriptor–Embedding Fusion for Glass Transition Temperature Prediction) concatenates 205 RDKit descriptors (RDKit205) with a frozen 384-dimensional ChemBERTa embedding (ChemBERTa384) and maps the 589-dimensional vector to Tg with an ExtraTreesRegressor. It was evaluated on 10,065 identity-resolved records of a polyimide-oriented dataset under three leakage-safe protocols: IID Group-Safe (IID, independent and identically distributed), Scaffold OOD (OOD, out-of-distribution), and Similarity OOD (T = 0.90). The model was selected on validation evidence and frozen before the final-test sets were opened. In the locked final test, CDEF-Tg reached a macro mean absolute error (MAE) of 48.84 °C, versus 50.17 °C (RDKit205 alone) and 54.33 °C (ChemBERTa384 alone). Group-aware bootstrap analyses separated CDEF-Tg from RDKit205 alone in MAE only under Similarity OOD and showed no MAE advantage over the comparator RDEF-Tg. Additional validation-only controls showed a lower macro MAE for a Morgan-fingerprint partner than for CDEF-Tg (49.11 versus 53.15 °C), and ChemBERTa384 lowered LightGBM error; the ExtraTrees ordering was stable across random states (split seeds were not varied). The results suggest a modest, protocol-dependent benefit within this dataset; the additional analyses provide descriptive evidence.
返回资讯频道