Airborne Microplastics in Spanish Schools: Abundance, Morphology, Polymer Composition and Aerodynamic Size in Urban and Peri-Urban Settings

发布时间:2026-11-07 | 来源:MDPI Polymers | 作者:Eugenia Battellocchi Garcia, María José Gómez, María Dolores Hernando Guil, Laura Cortés Corrales, C

Airborne microplastics (MPs) are emerging contaminants of concern in school environments, where children may experience prolonged exposure. This study assessed

Airborne microplastics (MPs) are emerging contaminants of concern in school environments, where children may experience prolonged exposure. This study assessed airborne MPs at three Spanish schools located in contrasting settings: a dense urban area in Madrid (A), a residential area in Almería (B), and an agricultural peri-urban area in Almería surrounded by greenhouses (C). An additional simultaneous indoor–outdoor comparison was performed at School B. Air samples were collected using active samplers with 25 µm stainless-steel meshes, and particles were characterised by stereomicroscopy, µ-FTIR spectroscopy, FESEM, and FTIR. Fibres were the predominant morphology, and polyethylene terephthalate (PET) was the most abundant synthetic polymer. School A showed the highest abundance of synthetic fibres, while polymer composition differed significantly among schools (χ2 (12) =41.77, p < 0.0001). Indoor samples contained more particles than outdoor samples, although natural-to-synthetic proportions were similar; PP, PA, and PE contributed relatively more indoors, whereas PET predominated outdoors. Only 0.45% and 0.13% of particles fell within the <10 µm and <4 µm estimated aerodynamic-size ranges, respectively, all being fibres. Overall, airborne MP occurrence varied with location and indoor–outdoor setting, while selected PET and PP fibres showed polymer-dependent surface and chemical alteration.

返回资讯频道