Comprehensive Study on Structural, Optical, Electrical and Thermal Properties of HPMC/PEG-Li2SO4 Solid Polymer Blend Electrolytes

发布时间:2025-12-31 | 来源:Semantic Scholar | 作者:Ali Adil Abbas; Aseel A. Kareem; A. R. Polu; Hani K. Ismail; Yosef Jazaa; Sun Theo Constan Lotebulo

ABSTRACT In this study, high-performance solid polymer electrolytes (SPEs) with different compositions were investigated for next-generation lithium-based energ

ABSTRACT In this study, high-performance solid polymer electrolytes (SPEs) with different compositions were investigated for next-generation lithium-based energy storage and flexible electronics technology applications. The SPE films were prepared by the solution casting method using hydroxypropyl methylcellulose (HPMC), polyethylene glycol (PEG), and lithium sulfate (Li2SO4). The obtained films were flexible and transparent, hence suitable for structural, optical, electrical, and thermal characterizations. The XRD pattern of HPMC indicated a broad peak at 2θ ≈ 20°, while the films HPMC/PEG- Li2SO4 showed sharp peaks assigned to the crystalline nature of Li2SO4. Fourier-transform infrared (FTIR) spectra confirmed O–H vibrations at 3484 cm− 1 and sulfate (SO42−) bands near 1056 cm− 1. UV–Vis analysis demonstrated that the strong absorption peak at 243 nm for HPMC/PEG and HPMC/PEG-10 wt.% Li2SO4 was accompanied by additional peaks at 230, 340, and 380 nm for HPMC/PEG-20 wt.% Li2SO4. The optical band gap decreased from 5.5 eV for pure HPMC to 2.1, 1.8, and 1.5 eV with addition of PEG and Li2SO4. AC conductivity improved with increasing frequency, showing an enhanced ionic conductivity for the 10 and 20 wt.% Li2SO4 compositions. TGA proved thermal stability up to 330°C while DSC showed Tg shifting to lower temperatures upon the addition of Li2SO4. GRAPHICAL ABSTRACT

返回资讯频道