Functional chitosan/poly(vinyl alcohol) biomembranes cross-linked with citric acid for efficient CO 2 /CH 4 separation

发布时间:2026-11-10 | 来源:RSC Applied Polymers | 分类:CA | 作者:RSC Applied Polymers

Chitosan (CS)/poly(vinyl alcohol) (PVA) biomembranes cross-linked with citric acid (CA) were developed to investigate the influence of composition and thermal c

Chitosan (CS)/poly(vinyl alcohol) (PVA) biomembranes cross-linked with citric acid (CA) were developed to investigate the influence of composition and thermal cross-linking conditions on their physicochemical properties and CO2/CH4 separation performance. Membranes with varying CA contents (25–57 wt%) and cross-linking times (1–3 h) were prepared and characterised in terms of morphology, structure, surface properties, thermal behaviour, water interaction, and mechanical performance. The results indicate that membrane properties were governed by the balance between network formation and the availability of functional groups. Among the compositions studied, 40 wt% of CA provided the most favourable balance between structural integrity and functional group accessibility, whereas lower CA contents were associated with less developed networks and higher contents with potential network heterogeneities. A cross-linking time of 2 h was found to be sufficient to achieve network formation without inducing thermal degradation. Gas permeation results revealed a trade-off between permeability and ideal selectivity, with CO2 permeability values of 123, 182, and 205 Barrer, and ideal CO2/CH4 selectivities of 33, 30, and 24 for membranes containing 25, 40, and 57 wt% of CA, respectively. Analysis of the estimated transport parameters indicated that the apparent solubility of CO2 was substantially higher than that of CH4, whereas their diffusivities were of the same order of magnitude, suggesting that gas selectivity was governed primarily by differences in apparent solubility. All membranes reached the first Robeson upper bound. Overall, these findings highlight the potential of CS/PVA/CA biomembranes for CO2/CH4 separation under humid conditions, and the importance of tailoring CA content to balance permeability and selectivity.

返回资讯频道