Comparative study on the reinforcement bond performance and ecological properties of graphite tailings concrete and ordinary concrete

发布时间:2026-11-13 | 来源:Nature Scientific Reports | 作者:Qing-Long Zeng

This study investigates the feasibility of applying Graphite Tailings Concrete (GTC) in reinforced concrete structures. The bond performance of GTC was systemat

This study investigates the feasibility of applying Graphite Tailings Concrete (GTC) in reinforced concrete structures. The bond performance of GTC was systematically evaluated and compared with that of Normal Concrete (NC). The effects of concrete strength grades and reinforcement types were considered, with NC used as the benchmark. Through 24 central pull-out tests and life cycle assessment, the differences between the two concretes in terms of bond performance, constitutive relationship, failure mode, and environmental impact were comprehensively analyzed. The results indicate that, in terms of bond performance, the bond strength of GTC with ribbed reinforcement at the C40 grade decreased by 12.93% compared with NC, while the peak slip increased by 39.4%. When the strength grade increased to C60, the bond strength of the two concretes were basically equivalent, with a decrease of only 0.86%, and the increase in peak slip narrowed to 61.9%, indicating that a high-strength matrix can effectively suppress the negative effects of graphite tailings. In terms of failure mode, GTC and NC exhibited complete consistency. At the C40 grade, both concretes showed pull-out failure, while at the C60 grade, all ribbed reinforcement specimens exhibited yielding failure. Regarding the interfacial ultimate fracture energy, the value of GTC with ribbed reinforcement at the C60 grade increased by 33.3% compared with NC, demonstrating superior energy dissipation capacity. Environmental assessment results show that although all environmental impact indicators of GTC were slightly higher than those of NC, the increases were limited, and the GWP at the C60 grade was only 0.40% higher than that of NC.

返回资讯频道