Fabrication of Bicontinuous Emulsions Stabilized by Amphiphilic Poly(hexyl Methacrylate-co-Methacrylic Acid) Self-Assembly Aggregates

发布时间:2026-11-12 | 来源:MDPI Polymers | 作者:Tongtong Cao, Hao Du, Yuyun Yang, Yuhua Cao

A facile strategy for fabricating bicontinuous emulsions stabilized by an amphiphilic random copolymer, poly(hexyl methacrylate-co-methacrylic acid) (P(HMA-co-M

A facile strategy for fabricating bicontinuous emulsions stabilized by an amphiphilic random copolymer, poly(hexyl methacrylate-co-methacrylic acid) (P(HMA-co-MAA)), was developed. The copolymer in aqueous solutions with pH less than 9.0 could self-assemble to form aggregates, whose morphologies were characterized by transmission electron microscopy (TEM) and scanning electron microscopy (SEM). The wettability of the self-assembly aggregates at the oil–water interface was investigated through three-phase contact angle measurements, which demonstrated a clear pH-responsive transition. As pH decreased, the contact angle gradually increased. At pH 7.0 and 8.0, the contact angle approached 90°. Based on this property, the bicontinuous emulsions were successfully prepared by a direct mixing method utilizing caprylic/capric triglyceride (GTCC) as oil phase and 1.0% (w/v) P(HMA-co-MAA) aqueous solution with pH 7.0 and 8.0 as the aqueous phase. Furthermore, the effects of oil–water mass ratio, polymer concentration, and copolymer monomer ratio on the formation of bicontinuous emulsions were also systematically studied. The findings revealed that only the copolymer with the monomer ratio of 7:3 had the same wettability in both oil and aqueous phases at pH 7.0 and 8.0. These copolymer aggregates could rapidly adsorb at the interface and produce a “soft jamming” effect, thereby effectively inhibiting phase separation.

返回资讯频道