Fano resonances in plasmonic gold gratings within a coupled-oscillator and diffraction framework

发布时间:2026-11-13 | 来源:Nature Scientific Reports | 作者:Mahdieh Hashemi

Plasmonic gold gratings supporting Fano resonances are promising candidates for sensing, filtering, and surface-enhanced spectroscopy, yet the lack of a rigorou

Plasmonic gold gratings supporting Fano resonances are promising candidates for sensing, filtering, and surface-enhanced spectroscopy, yet the lack of a rigorous analytical framework connecting their coupled-oscillator description to grating diffraction physics has made it difficult to design structures tailored to specific applications. Here, we establish this connection for gold gratings on a silica substrate under transverse magnetic illumination, and derive analytical relations between the Fano asymmetry parameter and the oscillator parameters, which we use to interpret the geometry dependence of the line shape. We develop a two-oscillator model in which the continuum mode is driven directly by the external field and the discrete mode is excited through coupling, and show analytically that the Fano resonance emerges near the natural frequency of the discrete oscillator due to its \(\pi \) phase transition, while the overall spectral envelope follows the continuum oscillator. Intermediate values of oscillator damping produce asymmetric Fano profiles, with the asymmetry type (dip–peak or peak–dip) governed by the coupling strength: for real coupling a dip–peak profile arises when the discrete oscillator frequency exceeds that of the continuum, while for imaginary coupling the condition is reversed. Applying this framework to gold gratings, we identify the propagating zero-order diffraction as the continuum channel and evanescent higher diffraction orders beyond the Rayleigh wavelength as the discrete resonance, which appears as surface plasmon polaritons (SPPs) localized predominantly at the metal–substrate interface. Momentum matching and the phase of \(H_z\) are consistent with an SPP at this interface: the phase difference between the fields at the Fano dip and peak is nearly uniform along the interface and close to \(\pi /2\) , whereas on the air side it is not. Parametric sweeps show that the ribbon width changes the resonance type (antiresonance, asymmetric …

返回资讯频道