Non-fluorinated waterproof breathable polyvinyl chloride nanofiber membranes produced by mixed-level factorial design and statistical approach
发布时间:2026-11-13 | 来源:RSC Applied Polymers | 分类:PVC | 作者:RSC Applied Polymers
Electrospun nanofibers have emerged as promising materials for waterproof breathable membranes (WBMs). However, many commercial WBMs rely on per- and polyfluoro
Electrospun nanofibers have emerged as promising materials for waterproof breathable membranes (WBMs). However, many commercial WBMs rely on per- and polyfluoroalkyl substances (PFAS), which pose significant environmental and health concerns. Here, we develop polyvinyl chloride (PVC) nanofiber membranes as a PFAS-free alternative, exploiting the polymer's intrinsic hydrophobicity and mechanical robustness. A mixed-level factorial design coupled with statistical optimization was employed to investigate the effects of PVC concentration, applied voltage, and tip-to-collector distance on fiber diameter, water contact angle, and water droplet retention. Among 18 experimental conditions, membranes fabricated using 12 wt% PVC, 15 kV applied voltage, and a 100 mm tip-to-collector distance achieved the optimal balance of morphology and wettability, yielding a global desirability of 0.85. The optimized membrane exhibited uniform fiber morphology, tensile strength of 1.6 MPa, and thermal stability up to 250 °C. Performance evaluation demonstrated excellent waterproofness, withstanding a hydrostatic pressure of 698 mbar, while maintaining adequate breathability with a water vapor transmission rate of 1.8 kg m−2 day−1. These findings demonstrate that electrospun PVC nanofibers represent a promising PFAS-free platform for sustainable WBMs, offering a balance of environmental compatibility, waterproofness, and breathability through statistically guided process optimization.
返回资讯频道