Gel polymer electrolytes (GPEs) require high room-temperature ionic conductivity and stable electrochemical properties to replace conventional liquid electrolyt
Gel polymer electrolytes (GPEs) require high room-temperature ionic conductivity and stable electrochemical properties to replace conventional liquid electrolytes. In this study, the content of 3-(1-vinyl-3-imidazolio)propanesulfonate (VIPS) was varied from 0 to 10 wt.% in a fluorinated gel polymer electrolyte with a fixed poly(ethylene glycol) diacrylate (PEGDA) and 2,2,2-trifluoroethyl methacrylate (TFEMA) host. Adding 5 wt.% VIPS increased the temperature at which the gel lost 10% of its initial mass from 238 to 266 °C. Also at 25 °C, the ionic conductivity increased from 2.10 mS cm−1 for the VIPS-free gel to 4.88 mS cm−1 at 5 wt.% VIPS and the oxidative onset potential also improved from 4.80 to 5.15 V (vs. Li/Li+). The optimized GPE with 5 wt.%, named ZF-GPE-V5, shows stable lithium plating and stripping behavior over 1000 h. An LFP|ZF-GPE-V5|Li cell recovered 99.50% of its initial low-rate discharge capacity after operation at 1.0 C and retained 87.16% of its initial capacity after 200 cycles at 0.2 C. These results suggest that the appropriate application of zwitterion-functionalized monomers can serve as a bridging technology between conventional batteries and future all-solid-state batteries.
返回资讯频道