Polym. Chem., 2026, 17, 2603-2618 DOI: 10.1039/D6PY00139D,论文 Alain Tundidor-Camba, Ifeanyi S. Ibeto, Yennier Cruz, Fidel E. Rodriguez-Gonzalez, Pravin S. Shinde

Polym. Chem., 2026, 17, 2603-2618 DOI: 10.1039/D6PY00139D,论文 Alain Tundidor-Camba, Ifeanyi S. Ibeto, Yennier Cruz, Fidel E. Rodriguez-Gonzalez, Pravin S. Shinde, Ana L. Montero-Alejo, Claudio A. Terraza, Sree Laxmi, Akhilesh Upasani, Sergey Vasenkov, Joshua D. Moon, Kathryn E. O'Harra, C. Heath Turner, Jason E. Bara 结构与热表征确认了成功合成,并揭示了季铵化和离子液体添加后聚合物基质的逐步致密化,这通过d-间距、自由体积分数和机械刚度的降低得以证实。本RSS Feed内容(c)皇家化学学会